Is the Exponent 3/2 Justified in Analysis of Loading Curve of Pyramidal Nanoindentations
SCANNING, Vol. 34, pp 410–417, 2012.

par   M. Troyon , Fazilay ABBES , Jaime Alexis Garcia Guzman

Résumé :

Kaupp and Naimi-Jamal (2010) claimed that the analysis of published loading curves reveals the exponent 3/2 to the depth for nanoindentations with sharp pyramidal or conical tips. To demonstrate this, they plotted the load vs. the penetration depth to the power 3/2. We show, through examples, the authors’ assertion is not credible because the methodology used is misleading and it cannot be asserted that the exponent 3/2 has a universal validity that applies to all kinds of materials.